The lead-zinc tailings sand was replaced by ordinary proportion of 0%,20%,40%,60%,80% and 100% of the total mass of concrete fine aggregate to pour concrete specimens for testing γ-ray shielding performance,slump and compressive strength.The test results showed that with the increase of tailings sand content,the gamma ray absorption coefficient μ gradually increased,the better the shielding performance,and the slump decreased.When the displacement ratio increased to 80%,100%,the decrease of slump was more obviouse;compared with ordinary concr...